J0043/EPM/ethylene propylene rubber/Ethylene Propylene Copolymer/lubricant additive/

Brief Description
Type: Synthetic Rubbers Model Number: J0043 
Specifications
J0043/EPM/ethylene propylene rubber/Ethylene Propylene Copolymer/lubricant additive/

J0043/ethylene propylene rubber
EPM Ethylene Propylene Copolymer
VII
Viscosity Index Improver

 J0043/EPM/ethylene propylene rubber/Ethylene Propylene Copolymer/lubricant additive

description:

Ethylene propylene copolymer is polymerized by ethylene and propylene. It is primarily used in blending medium-grade internal combustion engine oils. The product is white transparent colloid. It is solid in normal temperature.


CHARACTERISTICS

Excellent thickening capacity

Excellent shear stability and thermal oxidation stability

Good compatibility with all functional additives and pour point depressants

Improve the low temperature property of oil

Good oil soluble


The indices of the products

ITEM

INDICE

TEST METHOD

Volatility, %

≤0.75

GB/T 6373 (Oven Method)

Ash Content, %

≤0.10

GB/T 4498 (Method A)

Ethylene Content, %

52.5-57.5

Q/SY JH C 104001

Vanadium Content, ppm

≤10

Q/SY JH C 104004

Mooney Viscosity ML (1+4)100 °C

30-40

GB/T 1232.1

Shearing Stability Index (SSI)

≤40-45

----


 

Packing: The product is packed in polypropylene plastic bags. Each bag weights 25 kilogram. Every 42 bags are packed in a wooden box. The net weight of each wooden box is 1.05 ton.

Storage: This product is non-flammable and non-explosive. It is table under normal temperature. In transportation and storage, keep the temperature not higher than 60°C. For long-term storage the suggested temperature is lower than 50°C. The dry, clean and ventilating warehouse is recommended.